Specification of X1CrMoTi182:
– X1CrMoTi182 is a high-strength steel grade with excellent mechanical properties and corrosion resistance.
– It has a high tensile strength, ranging from 680 MPa to 880 MPa.
– X1CrMoTi182 exhibits good ductility with a minimum elongation of 18%.
– It has a hardness ranging from 180 HBW to 250 HBW.
– The steel grade has a density of approximately 7.8 g/cm^3.
– X1CrMoTi182 is known for its exceptional toughness and impact resistance.
– It has a high fatigue strength, enabling it to withstand cyclic loading without failure.
– The steel grade has a low coefficient of thermal expansion, making it suitable for applications with temperature variations.
– X1CrMoTi182 demonstrates excellent corrosion resistance to a variety of environments, including acidic and marine conditions.
– It has a high resistance to pitting, crevice, and intergranular corrosion.
– X1CrMoTi182 is capable of retaining its mechanical properties at elevated temperatures.
– It has good weldability and can be readily fabricated into various components.

Chemical Composition of X1CrMoTi182:
– Carbon (C): 0.08% – 0.15%
– Silicon (Si): 0.40% maximum
– Manganese (Mn): 0.40% – 0.70%
– Phosphorus (P): 0.025% maximum
– Sulfur (S): 0.010% maximum
– Chromium (Cr): 1.00% – 1.50%
– Molybdenum (Mo): 0.90% – 1.10%
– Nickel (Ni): 0.80% – 1.10%
– Titanium (Ti): 0.20% – 0.35%
– Nitrogen (N): 0.015% maximum
– Iron (Fe): Balance